MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese VECTRA® 3310MT 30% Glass Filled, Medical Grade Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Description: 30% glass reinforced medical grade with higher temperature capabilities than 1310MT. Has established Drug and Master Device Files.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPa5 mm/min; ISO 527-2/1A
Flexural Modulus 14.0 GPaISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Melting Point 325 °CISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75-1, -2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Vectra® C130 Liquid Crystal Polymer (LCP), 30% Glass Reinforced
Celanese Thermx® CG933 NC010 PCT
Celanese VECTRA® 2310MT 30% Glass Filled, Medical Grade Liquid Crystal Polymer (LCP)
Celanese VECTRA® 1310MT 30% Glass Filled, Medical Grade Liquid Crystal Polymer (LCP)
Celanese VECTRA C130 LCP, 30% Glass Reinforced

PHCW77 / 46018

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.