MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R413 NT0705 Impact Modified Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes:

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Water Absorption 1.0 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 1.9 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaConditioned; ISO 527-2
 110 MPaDry; ISO 527-2
Elongation at Break 5.0 %Dry; ISO 527-2
 13 %Conditioned; ISO 527-2
Tensile Modulus 4100 MPaConditioned; ISO 527-2
 5500 MPaDry; ISO 527-2
Flexural Strength 73.0 MPaConditioned; ISO 178
 140 MPaDry; ISO 178
Flexural Modulus 2800 MPaConditioned; ISO 178
 4800 MPaDry; ISO 178
Poissons Ratio 0.40Dry; ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -40.0 °C
Dry; ISO 180
 9.00 kJ/m²
@Temperature -40.0 °C
Conditioned; ISO 180
 10.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 180
 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 180
 12.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 180
 21.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 180
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 76.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -40.0 °C
Dry; ISO 179/1eA
 5.00 kJ/m²
@Temperature -40.0 °C
Conditioned; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cm
@Thickness 0.750 mm
IEC 60093
Dielectric Strength 3.00 kV/mm
@Thickness 1.00 mm
IEC 60243
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
PLC 6; ASTM D495
Comparative Tracking Index 400 - 599 V
@Thickness 3.00 mm
IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 112 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
Melting Point 260 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 235 °CISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection Molding
Middle Barrel Temperature 280 - 310 °CInjection Molding
Front Barrel Temperature 280 - 310 °CInjection Molding
Nozzle Temperature 280 - 310 °CInjection Molding
Melt Temperature 285 - 305 °CInjection Molding
Mold Temperature 65.0 - 95.0 °CInjection Molding
Drying Temperature 80.0 °C
@Time 14400 sec
Injection Molding
 
Descriptive Properties
Suggested Max Regrind (%)25
UsesCable Ties
 Circuit Board Standoffs
 Clamps
 Clips
 Connectors
 Electrical/Electronic Applications
 Fasteners
 Housings
 Industrial Applications
 Terminal Blocks
 Wheels

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® R413H NT Impact Modified Nylon 66, Glass Filled
Ascend Performance Materials Vydyne® 49H Impact Modified Nylon 66
Ascend Performance Materials Vydyne® 47 NT Impact Modified Nylon 66
Ascend Performance Materials Vydyne® 41 NT Impact Modified Nylon 66
Asahi Kasei Xyron® X5402 PPE/PA

PZASCE9719 / 220822

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.