MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound 2FL24 Ethylene Tetrafluoroethylene Copolymer (ETFE)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: LNP LUBRICOMP 2FL24 compound is based on Ethylene Tetrafluoroethylene (ETFE) resin containing 20% glass fiber and 10% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/ccASTM D792
Density 1.80 g/ccASTM D792
Moisture Absorption 0.0100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 67.0 MPa5 mm/min; ISO 527
 69.0 MPa5 mm/min; ASTM D638
Elongation at Break 6.2 %5 mm/min; ISO 527
 6.5 %5 mm/min; ASTM D638
Tensile Modulus 5000 MPa1 mm/min; ISO 527
 6440 MPa5 mm/min; ASTM D638
Flexural Strength 89.0 MPa2 mm/min; ISO 178
Flexural Modulus 4760 MPa1.3 mm/min, 50 mm span; ASTM D790
 4980 MPa2 mm/min; ISO 178
Izod Impact Notched 488 JASTM D256
Izod Impact, Unnotched 1340 J/mASTM D4812
Izod Impact, Notched (ISO) 45.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 92.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 20.0 JASTM D3763
Impact Test 8.00 JMultiaxial Impact; ISO 6603
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 24.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 94.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 239 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 251 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 198 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 300 - 325 °C
Zone 3 325 - 340 °C
Melt Temperature 315 °CInjection Molding
Mold Temperature 90.0 - 120 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80654 / 288601

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.