Titanvene™ HD5120GB-B is a high density polyethylene copolymer with a narrow molecular weight distribution, which has been specially developed for packaging carbonated beverages and for other applications where very high environmental stress cracking resistance (ESCR) is required. Titanvene™ HD5120GB-B has very good organoleptic properties, which does not significantly transfer taste or odor to the packaged product. Titanvene™ HD5120GB-B contains high slip agent to reduce the forces required to seal and open the cap. Titanvene™ HD5120GB-B is characterized by excellent impact strength and creep resistance. Applications: Titanvene™ HD5120GB-B is specialized for bottle caps of non-carbonated beverages or other closures where very high ESCR and reduced sealing and opening forces are required. Information provided by Lotte Advanced Materials. |