MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Konson ZBEC-70 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 70% Zinc-dibenzyl- dithiocarbamate, 30% EPDM/EVA binder and dispersing agents

Use Characteristics: A nitrosamine free super accelerator Konson® ZBEC-70 is a fast action thiocarbamate accelerator which has not been found to produce any harmful cancer-causing materials. Konson® ZBEC-70 can be used as a primary or secondary accelerator both in natural and synthetic rubbers, e.g. EPDM, IR, SBR, NBR, IIR. Compared with conventional dithiocarbamate accelerators, Konson® ZBEC-70 has a high level of processing safety. In compounds containing thiazole or sulphenamide accelerators, Konson® ZBEC-70 has an activating effect. Appropriate matching dosage of Zinc oxide and sulfur when using, the aliphatic acid (e.g. stearic acid) is not necessary. When same molar dosages of ZBEC-70 are used, vulcanizates containing Konson® ZBEC-70 demonstrate similar modulus to other dithiocarbamates.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective ZBEC is assured.

Dosage levels: EPDM: Konson® ZBEC-70: 0.8-2.5 phr
Konson® S-80: 1.0-2.0 phr
Konson® MBT (MBTS)-80: 1.0-2.0 phr
Konson® CBS-80: 0.5-1.5 phr
NR, SBR, NBR: Konson® ZBEC-70: 0.8-2.0 phr
Konson® S-80: 1.0-2.0 phr
Konson® MBT (MBTS)-80: 0.5-3.0 phr.

Applications: Suitable for technical rubber articles based on NR, EPDM, IR, SBR, NBR or IIR. Particularly suitable for light or brightly colored rubber articles.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.26 g/cc0.0434 - 0.0455 lb/in³
Ash <= 0.50 %<= 0.50 %
Evaporation Loss <= 0.50 %<= 0.50 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °F
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn 10 - 11.5 %10 - 11.5 %
 
Descriptive Properties
AppearanceLight-yellow granules
Content= 97%ZDMC
Sieve residue= 0.5 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS008 / 256053

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.