MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Pomalux® WRX Polyoxymethylene copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Pomalux WRX (Wear resistant polyoxymethylene copolymer) is an internally lubricated acetal copolymer. It offers enhanced wear and abrasion resistance and lower coefficients of friction compared to Pomalux WR and is similarly formulated with a PFOA free permanent lubricant. Pomalux WRX offers enhanced wear and friction performance versus PTFE filled POMc without the risk of voids and inclusions that are commonly associated with compression molded and extruded PTFE filed POMc. Pomalux WRX offers high strength and stiffness and good chemical resistance making it an ideal material for load bearing and transmitting components where enhanced wear, abrasion and low friction performance are critical performance requirements such as gears, bearing, chain guides and other conveyor components. Product is available in natural (off white) and black. Other colors are available on a make to order basis.

Colors Available: Black; Natural

Attributes: Chemical Resistance; Stiffness; Abrasion Resistant; Food Contact; Strength; Wear Resistance

Shapes: Compression Sheet; Extruded Rod

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

New suppliers have been added for this product during the past 60 days.  

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Moisture Absorption 0.220 %
@Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaASTM D638
Flexural Modulus 2423 MPaASTM D790
Izod Impact, Notched 40.5 J/mResistance; ASTM D256
 101.4 J/mASTM D256
Coefficient of Friction, Dynamic 0.26ASTM D3702 Modified
Coefficient of Friction, Static 0.30ASTM D3702 Modified
K (wear) Factor 3.00 x 10-10 in³-min/ft-lb-hrASTM D3702 Modified
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 87.7 °CASTM D648
 
Descriptive Properties
Compression Sheet Sizing120" Length by 48" Width0.5", 0.75", 1.0", 1.25", 1.5", 1.75", 2.0"
 48" Length by 24" Width0.5", 0.75", 1.0", 1.25", 1.5", 1.75", 2.0"
 96" Length by 48" Width0.5", 0.75", 1.0", 1.25", 1.5", 1.75", 2.0"
Rod Sizing48" Length2.25", 2.5", 2.75", 3.0", 3.25", 3.5"
 96" Length2.0'", 2.25", 2.5", 2.75", 3.0", 3.25", 3.5"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEST887 / 297289

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.