MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei KibipolĀ® SSBR PR-303 Styrene - Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Balanced physical properties and fabricability, good transparency, dimensional stability, smooth. Applications: Vulcanization of shoe soles, raw rubber-colored shoe soles, and for rubber modification.

KIBIPOLĀ® SSBR is a copolymerization of styrene and butadiene, created via a solution polymerization process. Its polydispersity is much narrower than SBR, offers an excellent balance between physical properties and fabricability. It delivers good transparency, processability, smoothness, and dimensional stability with multi-colored, pure white, or transparent designs. It can be used for GPPS modification to obtain HIPS with high drop impact strength (FDI) and low gel content.

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Mooney Viscosity 40 - 5040 - 50ASTM D1646
 
Descriptive Properties
APHA Color (APHA)<=10ASTM D1209
Bale Weight (kg)35
BD/SM (%)54/46ASTM D1646
Wrapping Film (type)LDPE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHI9913 / 280814

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.