MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips EC6600 HIPS - High Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Rubber modified high impact polystyrene.

Applications:

  • Lithographic sheet
  • Printed toys and games
  • Point of purchase displays
  • Silk screen printing
Features:
  • Excellent printability
  • Matte surface finish
  • High heat distortion temperature
  • Good low temperature toughness

Information provided by Chevron Phillips

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D-792
Bulk Density 38.0 - 42.0 lb/ft³
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm24 hours; ASTM D-955
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 22.0 MPa2.0 in/min; 0.050" thickness; ASTM D-638
Elongation at Yield 60 %2.0 in/min; 0.050" thickness; ASTM D-638
Tensile Modulus 1.72 GPa2.0 in/min; 0.050" thickness; ASTM D-638
Flexural Strength 38.0 MPa0.1 in/min; 0.250" thickness; ASTM D-790B
Flexural Modulus 1.62 GPa0.1 in/min; 0.250" thickness; ASTM D-790B
Izod Impact, Notched 117 J/m
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D-256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
@Thickness 6.35 mm
ASTM D-648
Vicat Softening Point 104 °C
@Thickness 6.35 mm
Rate B; ASTM D-1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americas Styrenics EA6740 High Impact Polystyrene
Americas Styrenics EB6400 High Impact Polystyrene
Americas Styrenics EB6755 High Impact Polystyrene
Americas Styrenics EC6600 High Impact Polystyrene
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene

PCHEVD275 / 20769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.