MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP17HTDA-2 One component die attach epoxy system
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Not premixed and frozen
  • Paste consistency
  • Thermally conductive, electrically insulating
  • High compressive strength
Product Description: Master Bond EP17HTDA-2 is a one component, heat cured epoxy system for bonding, sealing, and die attach applications. It does not require any mixing and the curing temperature is 300-350°F. It is not premixed and frozen and has an unlimited working life at room temperature. It will cure in either 4-5 hours at 300°F or 3-4 hours at 350°F. To optimize properties, use one of the above cure schedules plus an additional 2-3 hours at 400°F. Its viscosity and flow allow it be an effective adhesive for die attach applications. EP17HTDA-2 bonds well to a wide variety of substrates such as metal, ceramics, plastics and composites. It has an impressive array of physical strength properties, particularly tensile modulus, compressive strength and glass transition temperature. The system is thermally conductive and electrically insulative. It is highly chemically resistant to water, acids, bases, solvents, fuels, and oils. It has superb electrical insulation along with good thermal conductivity. The service temperature range is from -80°F to +600°F. The standard color is off white. EP17HTDA-2 is recommended for specialty type applications where a high Tg is a critical factor in die attach applications.

Product Advantages:

  • Single component system
  • Thermally conductive, electrically insulative
  • Can withstand temperatures used in electronic packaging such as wire bonding
  • Dispenses well for die attach applications
  • Passes NASA low outgassing specifications

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/cc
Solids Content 100 %100 %
Viscosity >= 1.00e+6 cP>= 1.00e+6 cPpaste
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 90 - 9590 - 95
Tensile Strength 31.0 - 37.9 MPa4500 - 5500 psi
Tensile Modulus >= 7.58 GPa>= 1100 ksi
Compressive Strength 193 - 207 MPa28000 - 30000 psi
Adhesive Bond Strength 11.0 - 12.4 MPa1600 - 1800 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 25.0 µm/m-°C11.1 - 13.9 µin/in-°F
Thermal Conductivity 1.30 - 1.44 W/m-K9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 316 °C600 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
Glass Transition Temp, Tg 185 - 190 °C365 - 374 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  180 - 240 min
@Temperature 177 °C
3.00 - 4.00 hour
@Temperature 350 °F
Option 2 (plus 2-3 hours at 400°F)
 240 - 300 min
@Temperature 149 °C
4.00 - 5.00 hour
@Temperature 300 °F
Option 1 (plus 2-3 hours at 400°F)
 
Descriptive Properties
Die shear strength20-23 kg-f2 x 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5909 / 306798

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.