MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Vulkacit® Merkapto/C Vulcanization Accelerator
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Vulcanization is the conversion of a high molecular material from the plastic to the elastic state. One of the key chemical reactions in this process is that of rubber with sulfur. Sulfur vulcanization, widely used in the rubber industry, requires the use of vulcanization accelerators such as Vulkacit®. Vulcanization accelerators are not catalysts because they are part of the chemical reaction. The great variety of accelerators available is a result of their different influences on the vulcanization kinetics (scorch and cure time) and on physical properties such as tensile strength, elasticity or resistance to aging. In many cases, accelerators are combined to supply optimal processing and physical properties.

Key PropertiesMercapto acceleratorsvery fast accelerators giving a very broad plateau and good aging resistance.Sulfenamide acceleratorsfast but very safe accelerators providing a steep slope on the rheometer curve.Thiuram acceleratorsfast accelerators, especially for efficient or sulfurless cure.Dithiocarbamate acceleratorsvery fast accelerators used alone or as a booster for thiazole and sulfenamide cure systems.Amine acceleratorsspecial accelerators for extraordinary applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Volatiles <= 0.30 %ASTM D4571
Ash <= 0.50 %ASTM D 4574
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 174 °CInitial; ASTM D1519 A
 <= 184 °CFinal; ASTM D1519 A
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Appearanceyellowish white powder
Assay>94%ASTM D4936
Content1-2%Oil
Specifications<0.5%Sieve residue (0.063 mm), ASTM D5461

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY9141 / 209532

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.