MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 4026 Double Coated Urethane Foam Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive system for bonding to various types of surfaces for mounting, joining and holding.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milRelease Liner
 1140 microns45.0 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.275 MPa39.9 psiT Block, 1 in2 (6.45 cm2) Jaw Speed 2 in/min (50 mm/min)
 1.24 MPa180 psi
Elongation at Break 100 %100 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 7.87 - 11.8 kV/mm200 - 300 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0620 W/m-K0.430 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 104 °C219 °FLong Term
 193 °C379 °FShort Term
 
Descriptive Properties
Adhesive Type100
LinerPolyurethane Foam

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33936 / 168683

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.