MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Rogers Arlon T1012-R004-xx 0.012" Self-Fusing Silicone Rubber Tape
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: 1 inch wide, 12 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.

Design/Construction:

  • Interleave: 1 mil Polyester
  • Rubber: Self-fusing Silicone Rubber
  • Cross-section: 1" wide rectangular

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³Silicone Property; Arlon SQA-TMS-024
Water Absorption 0.10 %0.10 %Arlon SQA-TMS-016
Thickness 305 microns12.0 milRubber; Arlon SQA-TMS-012
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4646Silicone Property; ASTM D2240
Tensile Strength 8.839 MPa1282 psiSilicone Property; ASTM D412
Elongation at Break 678 %678 %Silicone Property; ASTM D412
Peel Strength 0.403 kN/m2.30 pliBond Strength; Arlon SQA-TMS-015
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 39.4 kV/mm1000 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 204 °C400 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 21.1 °C
12.0 Month
@Temperature 70.0 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARL9851 / 149004

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.