MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: TOTAL Petrochemicals Polypropylene LX5 02-15 is an experimental grade of isostatic polypropylene copolymer produced via TOTAL proprietary metallocene catalyst technology.

Benefits. LX5 02-15 produces films with excellent heat seal performance and outstanding optical properties.

FDA. LX5 02-15 is cleared for food contact under Title 21 CFR Section 177.1520(c) 3.2a.

Recommended Applications. LX5 02-15 is an excellent material for use as a heat sealable layer un production of coextruded biaxially oriented films due to its good processing, excellent optics, very low extractables, low seal initiation temperature and exceptional hot tack seal strength properties.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.895 g/ccASTM D1505
Melt Flow 12 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 48.0 MPaASTM D638
Elongation at Break 800 %ASTM D638
Heat Seal Strength Initiation Temperature 221 °F
 
Thermal PropertiesOriginal ValueComments
Melting Point 119 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 0.30 %ASTM D1003
Gloss 96 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 218 - 274 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Novolen® 3520 L Polypropylene
Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion
Lushan M-10H Adhesive Resin for Multi-layer Sausage Casing film
Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film
Lushan M-10A Adhesive Resin for Multi-layer Sausage Casing film

PTOTAL842 / 130567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.