MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ COLORCOMP™ Compound EX14001 Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP COLORCOMP EX14001 compound is based on unfilled Polyetherimide (PEI) resin. Added features of this grade include: Easy Molding.

Features: Aesthetics and Appearance,Custom Color,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psi50 mm/min; ISO 527
Tensile Strength, Yield 105 MPa15200 psi50 mm/min; ISO 527
Elongation at Break 60 %60 %50 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 3.20 GPa464 ksi1 mm/min; ISO 527
Flexural Strength 160 MPa23200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 3.30 GPa479 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 390 - 400 °C734 - 752 °F
Zone 2 370 - 390 °C698 - 734 °F
Zone 3 380 - 400 °C716 - 752 °F
Melt Temperature 360 - 400 °C680 - 752 °FInjection Molding
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
 
Descriptive Properties
Screw speed (Circumferential speed)0.2-0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80555 / 288502

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.