MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EN 1.0116 High Manganese, Structural, Hot Rolled, Quality Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: Composition Note: N max na if Al >= 0.020

Key Words: EN 10025(90)A1(93) 1.0116. Similar to AISI 1513, UNS G15130
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³Estimated by MatWeb from similar grade
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  320 - 470 MPa
@Thickness 200 - 250 mm
46400 - 68200 psi
@Thickness 7.87 - 9.84 in
 340 - 470 MPa
@Thickness 63.0 - 80.0 mm
49300 - 68200 psi
@Thickness 2.48 - 3.15 in
 340 - 470 MPa
@Thickness 3.00 - 16.0 mm
49300 - 68200 psi
@Thickness 0.118 - 0.630 in
 340 - 470 MPa
@Thickness 3.00 - 16.0 mm
49300 - 68200 psi
@Thickness 0.118 - 0.630 in
 360 - 510 MPa
@Thickness <=1.00 mm
52200 - 74000 psi
@Thickness <=0.0394 in
 360 - 510 MPa
@Thickness <=1.00 mm
52200 - 74000 psi
@Thickness <=0.0394 in
Tensile Strength, Yield  175 MPa
@Thickness 200 - 250 mm
25400 psi
@Thickness 7.87 - 9.84 in
 215 MPa
@Thickness 63.0 - 80.0 mm
31200 psi
@Thickness 2.48 - 3.15 in
 235 MPa
@Thickness 3.00 - 16.0 mm
34100 psi
@Thickness 0.118 - 0.630 in
 235 MPa
@Thickness <=1.00 mm
34100 psi
@Thickness <=0.0394 in
 235 MPa
@Thickness 3.00 - 16.0 mm
34100 psi
@Thickness 0.118 - 0.630 in
 235 MPa
@Thickness <=1.00 mm
34100 psi
@Thickness <=0.0394 in
Elongation at Break  15 %
@Thickness <=1.00 mm
15 %
@Thickness <=0.0394 in
Transverse
 15 %
@Thickness <=1.00 mm
15 %
@Thickness <=0.0394 in
Transverse
 17 %
@Thickness <=1.00 mm
17 %
@Thickness <=0.0394 in
Longitudinal
 17 %
@Thickness <=1.00 mm
17 %
@Thickness <=0.0394 in
Longitudinal
 21 %
@Thickness 200 - 250 mm
21 %
@Thickness 7.87 - 9.84 in
Longitudinal
 21 %
@Thickness 200 - 250 mm
21 %
@Thickness 7.87 - 9.84 in
Transverse
 22 %
@Thickness 63.0 - 80.0 mm
22 %
@Thickness 2.48 - 3.15 in
Transverse
 24 %
@Thickness 63.0 - 80.0 mm
24 %
@Thickness 2.48 - 3.15 in
Longitudinal
 24 %
@Thickness 3.00 - 16.0 mm
24 %
@Thickness 0.118 - 0.630 in
Transverse
 24 %
@Thickness 3.00 - 16.0 mm
24 %
@Thickness 0.118 - 0.630 in
Transverse
 26 %
@Thickness 3.00 - 16.0 mm
26 %
@Thickness 0.118 - 0.630 in
Longitudinal
 26 %
@Thickness 3.00 - 16.0 mm
26 %
@Thickness 0.118 - 0.630 in
Longitudinal
Modulus of Elasticity 200 GPa29000 ksiEstimated by MatWeb from similar grade
Poissons Ratio 0.290.29Estimated by MatWeb from similar grade
Shear Modulus 80.0 GPa11600 ksiEstimated by MatWeb from similar grade
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmEstimated by MatWeb from similar grade
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FEstimated by MatWeb from similar grade
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FEstimated by MatWeb from similar grade
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FEstimated by MatWeb from similar grade
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.17 %<= 0.17 %
Iron, Fe >= 98.4 %>= 98.4 %As Balance
Manganese, Mn <= 1.4 %<= 1.4 %
Phosphorus, P <= 0.035 %<= 0.035 %
Sulfur, S <= 0.035 %<= 0.035 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1035 Steel, cold drawn, high temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1035 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
AISI 1010 Steel, cold drawn
AISI 1035 Steel, cold drawn, high temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1035 Steel, as cold drawn, 50-75 mm (2-3 in) round

M9ZE10116 / 232248

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.