MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Johnson Matthey Argo-braze™ 502 Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Argo-braze™ 502 is a specialized cadmium free silver-copper-zinc-nickel brazing filler metal with good flow and melting characteristics.

Nickel is a component of the filler metal’s composition, this being present to enhance its wetting and bonding properties on tungsten carbide. It is suitable for use on carbide tips where the largest dimension does not exceed 20 mm.

Argo-braze™ 502 can be used to braze 300 series stainless steel where it offers a high degree of protection against interfacial corrosion. It can also be used on the 400 series materials, but it does not offer the same level of protection against interfacial corrosion as on the 300 series materials.

Argo-braze™ 502 will fill joint gaps of between 0.075mm and 0.20mm at brazing temperature.

Argo-braze™ 502 can be used on stainless steel, mild steel, tungsten carbide and non-ferrous alloys. It should be noted that on 400 series stainless steels freedom from interfacial corrosion cannot be guaranteed. One of its principal uses is as a filler metal for brazing tungsten carbide tools.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 660 - 705 °C
Solidus 660 °C
Liquidus 705 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 20 %
Nickel, Ni 2.0 %
Silver, Ag 50 %
Zinc, Zn 28 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Argo-braze™ 56 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 60 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 60V Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 61V Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 632 Silver Brazing Filler Metal

NJMMJ9717 / 186118

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.