MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Promethium, Pm
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Most Property Data Below Is Estimated.

Physical Form: Silver-Metal; Hexagonal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.264 g/cc0.2624 lb/in³Alpha-Phase
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 145145Longest-Lived Isotope (1995)
Atomic Number 6161
X-ray Absorption Edge 0.27425 Å0.27425 ÅK
 1.66837 Å1.66837 ÅLI
 1.76581 Å1.76581 ÅLII
 1.91888 Å1.91888 ÅLIII
Ionic Radius 0.979 Å0.979 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 6363
Tensile Strength, Ultimate 160 MPa23200 psi
Tensile Strength, Yield 70.0 MPa10200 psi
Elongation at Break 25 %25 %
Tensile Modulus 50.0 GPa7250 ksi
Bulk Modulus 33.0 GPa4790 ksi
Poissons Ratio 0.280.28
Shear Modulus 18.0 GPa2610 ksi
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 53.0 J/g22.8 BTU/lb
CTE, linear 9.00 µm/m-°C5.00 µin/in-°Falong a-axis
 16.0 µm/m-°C8.89 µin/in-°Falong c-axis
 11.0 µm/m-°C
@Temperature 20.0 °C
6.11 µin/in-°F
@Temperature 68.0 °F
Bulk
Specific Heat Capacity 0.188 J/g-°C0.0449 BTU/lb-°F
Thermal Conductivity 17.9 W/m-K124 BTU-in/hr-ft²-°F
Melting Point 1042 °C1908 °F
Boiling Point 3000 °C5430 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 
Component Elements PropertiesMetricEnglishComments
Promethium, Pm 100 %100 %
 
Descriptive Properties
CAS Number7440-12-2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americium, Am
Silver, Ag
Aluminum, Al
Palladium, Pd
Neptunium, Np

AMEPm00 / 82

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.