MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Victrex APTIV™ 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Categories: Polymer; Film; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: APTIV™ 1100 series films are the mineral filled semi-crystalline films made from VICTREX™ PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom. APTIV 1100 has a combination of properties providing high temperature performance, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen free and ease of processing. APTIV 1100 series provides a higher modulus and lower coefficient of linear thermal expansion over the APTIV 1000 series.
    Applications:
  • Electrical insulation Printed circuit substrates
  • High temperature labels
  • Flexible surface heaters
  • Pressure sensor membranes
  • Acoustic speaker diaphragms and voice coils
  • Proven temperature resistance to use of lead free solders
Certification: APTIV film is FDA and EU approved for food contact and is RoHS compliant.
    Features:
  • High heat resistance
  • Broad chemical resistance
  • Excellent barrier properties
  • Low moisture absorption
  • High strength and toughness
  • Stable, excellent electrical insulation properties
  • Good flammability performance without use of flame retardant additives
  • Inherently halogen free
  • Radiation resistance
  • Low smoke and toxic gas emission
  • Excellent hydrolysis resistance
  • Excellent acoustic properties
  • High purity
  • Light weight
  • Recyclable
  • Easy to process – can be laminated to other materials, thermoformed, metallized, coated, printed, stamped and die cut, welded and heat sealed and coated.
  • Improved thermal conductivity over APTIV 1000 film
Surface Finishes: Standard surface finish is matte/matte.

Custom Finishing (Slitting and Surface Treatment): The slitter capability in the APTIV film facility allows custom lengths and widths down to 45 mm to be produced. Widths below 45 mm are available on request. Surface treatment by atmospheric plasma process of the film is also available by request taking the surface energy of the treated APTIV film surface to greater than 55 dynes per cm.

Compliance:
APTIV 1100 film is approved for Food Contact Use:
APTIV 1100 film is compliant with the compositional requirements of FDA 21 CFR 177.2415.
APTIV 1100 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC.
APTIV 1100 film complies with the requirements of RoHS
European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive.
APTIV 1100 film is inherently halogen free in accordance with IEC61249-2-21.

Secondary Processes:
APTIV 1100 film can easily be subjected to a range of secondary process operations, which allow designers and engineers to obtain the benefits of APTIV film properties in a variety of forms.

  • Surface treatment
  • Slitting
  • Adhesion
  • Die cutting and stamping
  • Coatings
  • Thermal lamination
  • Heat welding and heat sealing
  • Thermoforming
  • Metallisation
  • Printing
  • Laser marking and machining

    Property data reported herein was measured on 50 micron film. The films are available in thicknesses from 12 microns up to 125 microns.

Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/cc
@Temperature 23.0 °C
ISO 1183
Moisture Absorption at Equilibrium 0.090 %
@Temperature 23.0 °C,
Time 86400 sec
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD >= 10 %ISO 527
 >= 5.0 %
@Thickness 0.0250 mm
ISO 527
 >= 10 %
@Thickness 0.0250 mm
ISO 527
Film Elongation at Break, TD <= 10 %ISO 527
 <= 10 %
@Thickness 0.100 mm
ISO 527
 <= 10 %
@Thickness 0.100 mm
ISO 527
Tensile Modulus 4.50 GPaTD; ISO 527
 5.50 GPaMD; ISO 527
 4.50 GPa
@Thickness 0.100 mm
TD; ISO 527
 4.50 GPa
@Thickness 0.0250 mm
TD; ISO 527
 5.00 GPa
@Thickness 0.100 mm
MD; ISO 527
 5.50 GPa
@Thickness 0.0250 mm
MD; ISO 527
Tear Strength 28.0 pliMD; ISO 6383-1
 34.0 pliTD; ISO 6383-1
Film Tensile Strength at Break, MD 90.0 MPaISO 527
 70.0 MPa
@Thickness 0.0250 mm
ISO 527
 90.0 MPa
@Thickness 0.100 mm
ISO 527
Film Tensile Strength at Break, TD 90.0 MPaISO 527
 70.0 MPa
@Thickness 0.0250 mm
ISO 527
 90.0 MPa
@Thickness 0.100 mm
ISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
@Temperature 23.0 °C
100V; ASTM D257
Dielectric Constant 3.5
@Frequency 1e+7 Hz,
Temperature 23.0 °C
Dielectric Strength 200 kV/mm
@Temperature 23.0 °C
1/4 inch electrode; ASTM D149
Dissipation Factor 0.0010
@Frequency 1e+7 Hz,
Temperature 23.0 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°CMD, below Tg; ASTM D696
Thermal Conductivity 0.610 W/m-KThrough Plane; ASTM E1461
 1.30 W/m-KIn-Plane; ASTM E1461
Shrinkage, MD <= 0.50 %
@Temperature 200 °C
TM-XV-84
Shrinkage, TD <= 0.50 %
@Temperature 200 °C
TM-XV-84
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA YesSee notes for details.
 
Descriptive Properties
Puncture Strength5 kJ/m²MD/TD, Def Stan 81-75; 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ WG102 Polyaryletherketone
Saint-Gobain Rulon® 123 Bearing/Seal PTFE
Avient Trilliant™ HC HC6200-5002 XR Grey Polyamide 12 (Nylon 12)
Avient Trilliant™ HC HC6200-5001 XR Grey High Denisty Polyamide 12 (Nylon 12)
VICTREX™ PEEK 150CA30 30% Carbon Fiber Reinforced

PVICTA47a / 171868

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.