Silvaloy A45 FC is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is also used for brazing in electrical industry and for brazing brass parts such as ships, piping, band instruments and lamps. Generally, the joint strength of Silvaloy A45 FC will surpass the strength of the base metals.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies). |