MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives 810 Low Read-Through (LRT) Acrylic Adhesive with Accelerator 20GB
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: LORD® 810 Low Read-Through (LRT) acrylic adhesive when cured with LORD Accelerator 20GB creates a flexible adhesive system for bonding metals, such as aluminum, galvanized steel and CRS, and engineered plastics, such as PC-ABS. LORD 810 adhesive in combination with LORD Accelerator 20GB delivers fast cure speed and strong bonding with minimal bondline read-through (BLRT). LORD Accelerator 20GB allows precise control of the adhesive bondline thickness due to its content of glass beads. LORD 810 adhesive is flammable. Do not store or use near heat, sparks or open flame.

Features: bonds thin and flexible substrates with little to no bondline read-through. requires little or no substrate preparation for bonding metals and plastics. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility. resists dilute acids, alkalis, solvents, greases, oils and moisture; provides excellent resistance to indirect UV exposure and weathering. performs at temperatures from -40°F to +300°F (-40°C to +149°C).

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 - 0.971 g/cc0.0338 - 0.0351 lb/in³
Brookfield Viscosity 40000 - 130000 cP
@Temperature 25.0 °C
40000 - 130000 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040Cured
 6969Post-Baked
Tensile Strength at Break 5.80 MPa841 psiCured
 14.4 MPa2090 psiPost-Baked
Elongation at Break 22 %22 %Post-Baked
 190 %190 %Cured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 43.0 °C109 °FCured
 58.0 °C136 °FPost-Baked
Flash Point 15.0 °C59.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 20.0 - 25.0 min
@Temperature 21.0 °C
20.0 - 25.0 min
@Temperature 69.8 °F
Time to Handling Strength, 50 psi shear
Working Life 8.00 - 12.0 min
@Temperature 21.0 °C
8.00 - 12.0 min
@Temperature 69.8 °F
 
Descriptive Properties
AppearanceBlack Paste
 GreyCured Appearance
 Grey PasteMixed Appearance
Mix Ratio1.1 to 1by weight, adhesive to accelerator
 2 to 1by volume, adhesive to accelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9110 / 232498

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.