MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Gichem GIPRENE Sh 70 TPE Flame Retardant - Standard Type  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Information provided by GICHEM Gruppo Industriale Chimico

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³in distilled water; ISO R1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 727215s; ASTM D2240
Tensile Strength, Yield 7.00 MPa1020 psitraction speed 250 mm/min; ISO R37
Elongation at Break >= 400 %>= 400 %traction speed 250 mm/min; ISO R37
100% Modulus 2.70 MPa
@Strain 100 %
392 psi
@Strain 100 %
traction speed 250 mm/min; ISO R37
300% Modulus 5.00 MPa
@Strain 300 %
725 psi
@Strain 300 %
traction speed 250 mm/min; ISO R37
Tear Strength Test 3030[ MPa ] Type DIE C; ISO R34
Compression Set 45 %
@Temperature 100 °C
45 %
@Temperature 212 °F
(22h / 100°C / 25%); ASTM D395 B
Tensile Set 11 %11 %( 10min / 100% deform.); ISO R2285
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
Oxygen Index 27.5 %27.5 %ASTM D2863
 
Descriptive Properties
HCL Emission, %4

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 451-87 Thermoplastic Rubber

PGICH64 / 41881

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.