MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay AVIMID® N Polyimide Composite
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: AVIMID® N is a high temperature, post-curable, 775°F (413°C) Tg thermoplastic polyimide composite with wet service capability up to 630°F (332°C) and dry service capability of 700°F (370°C). AVIMID N has the industry’s best thermal oxidative resistance of all organic matrices and is the preferred product when high temperature durability is needed. It is a very tough composite system and has favorable dielectric properties making it well suited for missile and turbine engine applications. AVIMID N was formulated to be a non-MDA, high temperature composite that would allow the use of typical safety/health procedures and personal protection equipment (PPE). It can be compression molded into low void parts to meet demanding aerospace requirements or alternatively processed in a vacuum bag autoclave process to meet more flexible requirements usually seen in non-aerospace applications. AVIMID N is solution impregnated on a variety of fibers and fabrics that result in prepregs that retain their tack and drape for up to 6 days at 70°F (21°C). Tack can be regenerated or enhanced in a limited way by spraying the prepreg with ethanol. The prepreg has a shelf life of 12 months from date of manufacture when stored at 0°F (-18°C).

Features & Benefits:

  • Most thermal oxidatively stable polyimide composite
  • Post-curable Tg as high as 775°F (413°C)*
  • Non-MDA system; no carcinogenic components
  • Service temperature 630°F (332°C) wet and 700°F (370°C) dry
  • Tough, micro-crack resistant resin
  • Low and favorable dielectric properties
  • Autoclave or compression moldable
  • Shelf life of 12 months at 0°F (-18°C). 6 days at 70°F (21°C)
  • Specified for turbine engine and industrial use
Applications:
  • Turbine engine components
  • Missile components

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13800 psi
@Temperature 332 °C
90°, 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
 14500 psi
@Temperature 24.0 °C
90°, 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
 65100 psi
@Temperature 24.0 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 67000 psi
@Temperature 332 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 69400 psi
@Temperature 332 °C
wet, 16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 70000 psi
@Temperature 204 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 177000 psi
@Temperature 332 °C
0°, 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
 180000 psi
@Temperature 332 °C
0°, wet 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
Tensile Modulus 16.1 GPa
@Temperature 332 °C
90°, 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
 17.6 GPa
@Temperature 24.0 °C
90°, 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
 42.0 GPa
@Temperature 332 °C
wet, 16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 49.0 GPa
@Temperature 204 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 50.0 GPa
@Temperature 24.0 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 50.0 GPa
@Temperature 332 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F (413°C) *
 132 GPa
@Temperature 332 °C
0°, 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
 150 GPa
@Temperature 332 °C
0°, wet 10 ply graphite uniweave (G30-500), Tg = 775°F (°C) *
Flexural Strength 7000 psi
@Temperature 24.0 °C
6 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45)
 44000 psi
@Temperature 332 °C
wet, 16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
 53800 psi
@Temperature 332 °C
6 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45)
 99000 psi
@Temperature 332 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
 129000 psi
@Temperature 204 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
 213000 psi
@Temperature 24.0 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
Flexural Modulus 49.0 GPa
@Temperature 332 °C
6 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45)
 54.0 GPa
@Temperature 24.0 °C
6 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45)
 101 GPa
@Temperature 332 °C
wet, 16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
 103 GPa
@Temperature 332 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
 103 GPa
@Temperature 204 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
 111 GPa
@Temperature 24.0 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 775°F (413°C) *
Compressive Strength 239 MPa
@Temperature 332 °C
wet, 16 ply graphite unidirectional uniweave (G30-500), Tg = 710°F (377°C) *
 363 MPa
@Temperature 332 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 710°F (377°C) *
 421 MPa
@Temperature 24.0 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F
 889 MPa
@Temperature 24.0 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 710°F (377°C) *
Compressive Modulus 48000 MPa
@Temperature 24.0 °C
16 ply graphite uniweave (G30-500), quasi-isotropic (0, 90, ±45), Tg = 775°F
 112000 MPa
@Temperature 24.0 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 710°F (377°C) *
Shear Modulus 5.60 GPaIn-plane, 16 ply graphite uniweave (G30-500), bias (±45), Tg = 785°F (418°C) *
Shear Strength 5600 psi
@Temperature 360 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 785°F (418°C) *
 6700 psi
@Temperature 316 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 785°F (418°C) *
 8900 psi
@Temperature 218 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 785°F (418°C) *
 12700 psi
@Temperature 24.0 °C
In-plane, 16 ply graphite uniweave (G30-500), bias (±45), Tg = 785°F (418°C) *
 14300 psi
@Temperature 24.0 °C
16 ply graphite unidirectional uniweave (G30-500), Tg = 785°F (418°C) *
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 332 °Cwet
 370 °Cdry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay AVIMID® R Polyimide Composite
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Evonik SOLIMIDE® AC-550 Polyimide Foam
Solvay AVIMID® RB Polyimide Composite
Arlon Electronic Materials 84N Polyimide Laminate and Prepreg

PCYTED075 / 180377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.