MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Copper, UNS C40800, OSO15 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability. Fabricated by blanking, stamping, and shearing.

Applications: electrical connectors.

Test specimen: flat products - 1mm thickness.

Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.86 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 69
Hardness, Rockwell 30T 31
Tensile Strength, Ultimate 310 MPa
Tensile Strength, Yield 105 MPa
@Strain 0.5 %
Elongation at Break 42 %In 50 mm
Modulus of Elasticity 110 GPaHard
Poissons Ratio 0.341
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 41.0 GPa
Shear Strength 235 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000466 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 160 W/m-K
@Temperature 20.0 °C
Melting Point 1038 - 1054 °C
Solidus 1038 °C
Liquidus 1054 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 450 - 675 °C
Hot-Working Temperature 830 - 890 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 95 %
Tin, Sn 2.0 %
Zinc, Zn 3.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper nickel 20%, UNS C71000, H04 Temper flat products
Copper nickel 20%, UNS C71000, H55 Temper flat products
Copper, UNS C40800
Copper, UNS C40800, H10 Temper flat products
Copper, UNS C40800, H08 Temper flat products

MC40800b4 / 11269

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.