MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Halar® 6012F ECTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Halar® 6012F is semi-crystalline fluoropolymer designed specifically for rotational molding and lining. Rotomolding is typically used to manufacture articles such as tanks, bottles and vessels whilst rotolining is used to coat pipes, fittings, valves, tanks and vessels.

Main features of Halar® 6012F are:
- Excellent chemical resistance
- Excellent permeation resistance
- Smooth surface finish
- Good flow
- Good thermal stability
- High purity
- Flame retardant

Applications: Bottles; Coating Applications; Pipe Coatings; Protective Coatings; Tanks; Valves/Valve Parts; Vessels

Features: Abrasion Resistant; Barrier Resin; Chemical Resistant; Flame Retardant; Good Flow; Good Surface Finish; Good Thermal Stability; High Purity; Non-Stick

Processing
- Halar® 6012F can be processed using normal rotomolding/rotolining techniques. In the case of rotomolding Halar® 6012F is initially introduced into a mold. This is then heated in an oven and maintained under rotation to achieve the desired mold shape. Finally, mold extraction and cooling are carried out to obtain the final item. In rotolining, the resin is directly fed inside the part to be lined. As in the case of rotomoldings, the part is then heated, maintained under rotation and finally cooled to obtain the lined article.

- Halar® 6012F can be used neat and without any further formulation. Substrate preparation, Halar® load, rotation parameters, oven temperature and time must all be well controlled to achieve defect free items.

Storage and Handling
- Halar® melt processable fluoropolymer resins can be stored without shelf life issues when kept in a clean and dry area at ambient temperatures. Opened containers should be tightly resealed to prevent dust contamination.

Safety and Toxicology
- Before using Halar® melt processable fluoropolymer resins consult the product Material Safety Data Sheet and follow all label directions and handling precautions. As with all fluoropolymer materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact, wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes. See Material Safety Data Sheet for detailed advice on waste disposal methods.

Packaging
- Halar® 6012F is packaged in 25 kg non-returnable drums. Each drum has two bag liners made of polyethylene resin.

Additional Technical Information
- For Material Safety Data Sheet or additional technical information consult your Solvay representative or the website: www.solvayspecialtypolymers.com

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccASTM D1505
Particle Size 300 - 500 µm
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPowder
ProcessingRotational Molding; Roto Lining

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4225 / 280025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.