Arnite® T AM1210 (P) is a PBT powder commercially available for selective laser sintering. The material is ideal for small series production via additive manufacturing in industrial applications such as automotive electronics.- Well-known material with dielectric properties
- PBT powder for selective laser sintering
Arnite® T AM1210 (P) has the same dielectric properties as material used in injection molding processes, making it a material engineers are familiar with and prepared to use. Developed for a wide sinter window. Arnite® T AM1210 (P) is environmentally friendly with a high reuse rate and is recyclable to the extent that the material can be brought back to the powder bed process. Key Benefits: - A well-known material that can be adopted quickly
- Excellent dielectric properties
- Easy to print
- Improved dimensional stability due to lower moisture uptake
- Less waste due to >60% reuse rate
- Recyclable: non-reusable material can be brought back to the powder bed process
Applications: - Connectors
- Automotive Electronics
- Electrical
- Lighting
Former DSM Engineering Plastics product line is now with Envalior. |
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |