MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Traid Villarroya TKG® FLON PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Excellent resistance to continuous service temperature up to 260°C.
  • Satisfactory low temperature resistance as low as -200°C.
  • Excellent chemical resistance
  • Excellent electrical insulation
  • Excellent slide and wear properties
  • Inherent flame retardant
Industry Applications:
  • Conveyor technology
  • Chemical plant engineering
  • Electrical and precision engineering
  • Food engineering
  • Medical industry

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.15 g/cc0.0777 lb/in³
Water Absorption <= 0.010 %<= 0.010 %ASTM D 570
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness >= 23.0 MPa>= 3340 psiISO 13000-2
Tensile Strength 22.0 MPa3190 psiASTM D 4894
Elongation at Break >= 200 %>= 200 %ASTM D 4894
Compressive Strength 5.00 MPa
@Strain 1 %
725 psi
@Strain 1 %
ASTM D 695
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D 257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D 257
Dielectric Constant 2.1
@Frequency 50.0 - 109 Hz
2.1
@Frequency 50.0 - 109 Hz
ASTM D 150
Dielectric Strength >= 80.0 kV/mm>= 2030 kV/inIn air; ASTM D 149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature 25.0 - 100 °C
72.2 µin/in-°F
@Temperature 77.0 - 212 °F
ASTM C 177
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C 177
Maximum Service Temperature, Air 260 °C500 °FShort term
 260 °C500 °FLong term
Glass Transition Temp, Tg -20.0 °C-4.00 °FDIN 53765
Flammability, UL94 V-0V-0DIN IEC 60995-11-10
 
Descriptive Properties
ColorWhite opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAID915 / 318876

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.