MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Melos Mecoline S TP 1001 F Halogen-free, thermoplastic, highly flame retardant sheathing compound
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, highly flame retardant sheathing compound for low and medium voltage cables

Compound class: Sheathing

Compound category: TP

Flame retardant: ATH

Standards: BS 6724; BS 7655 section 6.1 LTS 1 - LTS 4; CEI 20-11 M1 DIN EN 50363-8 TM7; DIN VDE 0276-604 HM4; DIN VDE 0281 part 14 TM7; IEC 60092-360 SHF 1; NF C 32-323; VDE 0207 part 24 HM 2, HM 4; VDE 0250 part 215 HM5

Typical applications: Halogen-free, low smoke, thermoplastic, highly flame retardant compound for the sheathing of low and medium voltage cables in General Installation applications.

Features: Flame retardant; Tear resistant; Halogen-free; Abrasion resistant; Low smoke

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccpressed plaques, 155°C / 5 min; DIN EN ISO 1183-1A
pH >= 6.5Corrosivity, Acid gas emission; IEC 60754-2
Melt Flow 11.5 g/10 min
@Load 21.6 kg,
Temperature 150 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55pressed plaques, 155°C / 5 min; DIN ISO 7619-1
Tensile Strength 13.8 MPaextruded tapes; IEC 60811-501
 4.83 MPa
@Temperature 100 °C,
Time 605000 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 10.67 MPa
@Temperature 70.0 °C,
Time 605000 sec
extruded tapes, Water purified; IEC 60811-404
 12.3 MPa
@Temperature 100 °C,
Time 21600 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 13.0 MPa
@Temperature 100 °C,
Time 864000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
 13.386 MPa
@Temperature 23.0 °C,
Time 86400 sec
extruded tapes, Water purified; IEC 60811-404
 15.1 MPa
@Temperature 120 °C,
Time 605000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
Elongation at Break 205 %extruded tapes; IEC 60811-501
 71.75 %
@Temperature 100 °C,
Time 605000 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 181.015 %
@Temperature 70.0 °C,
Time 605000 sec
extruded tapes, Water purified; IEC 60811-404
 195.98 %
@Temperature 120 °C,
Time 605000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
 202.13 %
@Temperature 23.0 °C,
Time 86400 sec
extruded tapes, Water purified; IEC 60811-404
 209.92 %
@Temperature 100 °C,
Time 864000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
 209.92 %
@Temperature 100 °C,
Time 21600 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
Penetration 3.0
@Temperature 80.0 °C,
Time 21600 sec
[%] Hot pressure test, extruded tapes; IEC 60811-508
 13
@Temperature 90.0 °C,
Time 21600 sec
[%] Hot pressure test, extruded tapes; IEC 60811-508
Tear Strength 10.5 kN/mextruded tapes; BS 6469:99.1
Abrasion 94[mm3], pressed plaques, 155°C / 5 min; DIN VDE 0472-605
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.80e+13 ohm-cm
@Temperature 20.0 °C,
Time 57600 sec
500V, pressed plaques, 155°C / 5 min; DIN VDE 0303-30
Dielectric Constant 3.96
@Frequency 1e+6 Hz,
Temperature 23.0 °C
1V, pressed plaques, 155°C / 5 min; IEC 60250
 5.04
@Frequency 1000 Hz,
Temperature 23.0 °C
1V, pressed plaques, 155°C / 5 min; IEC 60250
 5.44
@Frequency 50 Hz,
Temperature 23.0 °C
100V, pressed plaques, 155°C / 5 min; IEC 60250
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °C
Minimum Service Temperature, Air -29.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 170 °CTool
 160 - 170 °CMaximum mass temperature
Zone 1 90.0 - 110 °C
Zone 2 105 - 125 °C
Zone 3 120 - 140 °C
Zone 4 120 - 140 °C
Zone 5 130 - 150 °C
Adapter Temperature 135 - 155 °C
Head Temperature 140 - 160 °C
Drying Temperature 60.0 - 70.0 °C
Dry Time 4.00 - 6.00 hour
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 36 %pressed plaques, 155°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Conductivity<14 µS/cm-1pressed plaques, 155°C / 5 min, IEC 60754-2
Impact strengthPassat -25°C, extruded tapes, IEC 60811-506
NBS-smoke chamber test05:53Time to DS max., pressed plaques, 155°C / 5 min., ASTM E 662
 09:11Time to DS max., pressed plaques, 155°C / 5 min., ASTM E 662
 15DS max. (non-flaming), pressed plaques, 155°C / 5 min., ASTM 662
 208DS max. (non-flaming), pressed plaques, 155°C / 5 min., ASTM 662
ShrinkagePassat 70°C, extruded tapes, IEC 60811-508
Temperature index295°Cpressed plaques, 155°C / 5 min, ASTM D 2863 D
Toxicity index<1.1pressed plaques, 155°C / 5 min, NES 713
Water absorption0.13[mg/cm²], Water purified 24h at 23°C, extruded tapes, IEC 60811-404
 0.15[%], Water purified 24h at 23°C, extruded tapes, IEC 60811-404
 1.62[mg/cm²], 24h at 70°C, extruded tapes, IEC 60811-402

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS000 / 296107

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.