MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Brandenburger Supratherm T High Temperature Insulation Material  (discontinued **)
Categories: Ceramic

Material Notes: This tightly compressed fibre cement material is well suited as an asbestos substitute

Information provided by Brandenburger Isoliertechnik GmbH&Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³
Water Absorption <= 15 %<= 15 %24 hrs; DIN 53 495
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 24.0 MPa3480 psiEN 63
Compressive Strength 100 MPa14500 psiEN ISO 604
 60.0 MPa
@Temperature 300 °C
8700 psi
@Temperature 572 °F
ISO 604
 75.0 MPa
@Temperature 200 °C
10900 psi
@Temperature 392 °F
EN ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 µm/m-°C
@Temperature 20.0 °C
2.78 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.320 W/m-K2.22 BTU-in/hr-ft²-°FDIN 52 612
 0.400 W/m-K
@Temperature 200 °C
2.78 BTU-in/hr-ft²-°F
@Temperature 392 °F
DIN 52612
Maximum Service Temperature, Air 500 °C932 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brandenburger Supratherm H High Temperature Insulation Material
Brandenburger Supratherm HT 175 High Temperature Insulation Material
Brandenburger Supratherm HT 4 High Temperature Insulation Material
Brandenburger Flexline Insulation
Brandenburger BRA-GLA Special Grade

PBRAND13 / 27726

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.