MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

KLJ Group KANATOL 200 Plasticizer
Categories: Fluid

Material Notes: Properties: DEP is a colourless, transparent oily liquid, slight aromatic odor

Application: As a solvent for nitro-cellulose and cellulose acetate in manufacturing of varnishes & paints. As fixative in fragrance/perfumes such as in aggarbatti. As alcohol denaturant. As a camphor substitute.

Chemical Name: Di Ethyl Phthalate

Molecular Formula: C 12 H14 O4

Molecular Structure: C 6 H 4 (C00C 2 H 5 ) 2

CAS Number: 84-66-2

UN. NO: 3082

EINECS NO.: 201-550-6

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.114 - 1.12 g/cc
@Temperature 27.0 °C
1.114 - 1.12 g/cc
@Temperature 80.6 °F
ASTM D1045-08
Viscosity 9.0 - 15 cP9.0 - 15 cPKLJ TM-P-13-97
Molecular Weight 222 g/mol222 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point 298 °C
@Pressure 0.101 MPa
568 °F
@Pressure 14.7 psi
IS 5298-05
Flash Point 160 °C320 °FCOC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.497 - 1.503
@Temperature 27.0 °C
1.497 - 1.503
@Temperature 80.6 °F
ASTM D1045-08
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %ASTM E203-08
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Acidity after heat treatment<0.05%180°C for 2 hrs, ISI-9591-03
Acidity as Acid<0.015%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<20Hazen, ASTM D1045-08
Content<0.02%Residual/Free Alcohol, KLJ TM-P-12-98
 >99.5%Ester Content, ASTM D1045-08
 >99.5%Plasticizing Ester by GLC, KLJ TM-P-12-98
 500-506 mg KOH/gmEster Value, ASTM D1045-08
Heat Stability35 Huat 150°C for 2 hrs, ISI-9591-03
Volatile Loss<0.2%110°C for 1 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKLJ236 / 284257

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.