MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3M HGS19K46 Glass Bubbles
Categories: Ceramic; Glass

Material Notes: 3M™ Glass Bubbles HGS19K46 are high-strength, low-density additives specially formulated to afford greater survivability than other lightweight additives under demanding downhole conditions. They are hollow glass microspheres made from water-resistant and chemically-stable soda-lime borosilicate glass. When drilling and cementing across highly depleted zones and weaker formations, low-density systems are required to prevent/ minimize problems associated with excessive overbalance conditions including fluid loss/lost circulation, differential sticking, minimal penetration rates, formation damage, and reduced well productivity. The use of 3M glass bubbles HGS19K46 as density reducing agents for drilling, completion, work-over fluids, and cement slurries offers the potential for
  • Reduced Non Productive Time (NPT)
  • Improved well integrity
  • Increased well productivity

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.460 g/cc0.460 g/ccTrue
Particle Size 20 µm20 µmAverage
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 131 MPa19000 psi80%
 
Descriptive Properties
Color, unaided eyeOff-white, powdery
CompositionSoda-lime-borosilicate glass
Packing factor58%bulk density to true particle density ratio
ShapeHollow spheres with thin walls

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMM40009C / 255387

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.