MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Ethyl Acetate, Urethane Grade Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 141-78-6

Product Description: Eastman™ Ethyl Acetate, Urethane Grade is a low-boiling, fast-evaporating solvent with a mild, pleasant odor. It is widely used in formulating printing inks, adhesives, and lacquers. It is a non- HAP solvent with excellent activity for most coating resins. Ethyl acetate is miscible with most organic solvents and can be used in cleaner blends for the removal of oils, grease, and soils. The chemical substances for this product are listed as Inert Ingredients Permitted for Use in Nonfood Use Pesticide Products, and in Food Use Pesticide Products with limitations, under the Federal Insecticide, Fungicide, and Rodenticide Act (FIFRA).

Application/Uses:

  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Misc. (Thinners and Purge Solvents)
  • Coatings - Transportation
  • Denaturant for ethyl alcohol
  • Graphic Arts - Flexographic and Gravure Printing Inks
Key Attributes:
  • Excellent solvent activity
  • Fast evaporation rate
  • High electrical resistance
  • Inert - Nonfood use
  • Low MIR value
  • Low surface tension
  • Mild odor
  • Non-HAP
  • Non-SARA
  • Readily biodegradable
  • Urethane grade

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³
Viscosity 0.50 cP0.50 cPLiquid
Molecular Weight 88.11 g/mol88.11 g/mol
Vapor Pressure  0.00173 bar
@Temperature 20.0 °C
1.30 torr
@Temperature 68.0 °F
 0.458 bar
@Temperature 55.0 °C
344 torr
@Temperature 131 °F
Surface Tension 23.9 dynes/cm23.9 dynes/cm
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 38.8 bar29100 torr
Critical Temperature 250.1 °C482.2 °F
Total Acid Number <= 0.0050<= 0.0050
 
Thermal PropertiesMetricEnglishComments
CTE, linear 134 µm/m-°C74.4 µin/in-°F
Melting Point -83.0 °C-117 °FFreezing Point
Boiling Point 75.5 - 78.5 °C168 - 173 °F
Flash Point -4.00 °C24.8 °FTag Closed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.37181.3718
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5233 / 222427

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.