MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Bergamid™ B700 UF black Polyamide 6 (Nylon 6), DAM
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/cc±0.03 g/cm³; DIN 53479
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa
@Temperature 23.0 °C
ISO 527-2/5
Elongation at Break 20 %
@Temperature 23.0 °C
ISO 527-2/5
Tensile Modulus 1500 MPa
@Temperature 23.0 °C
ISO 527-2/1
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.30 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 8.40 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Constant 7.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 45.0 kV/mmIEC 60243-1
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °CISO 3146
Maximum Service Temperature, Air 85.0 °CContinuous (GTP 50% Tensile); IEC 60216
 160 °CShort Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 190 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.800 mm
ALL; Internal Method
Glow Wire Ignition Temperature 960 °C
@Thickness 3.00 mm
0.8 mm wire; Ignition Temperature; IEC 60695-2-13
 
Descriptive Properties
FeaturesFlame Retardant
 Halogen Free
 Low (to None) Phosphorus Content
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
K-Value74.0 to 78.0No Standard; 96% H2SO4
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® C 50 H2 PA6, DRY
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Celanese Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Envalior Akulon® K225-KS (Cond.) Flame Retardant (Halogen free), Heat Stabilized Nylon 6 (North America)
NYCOA 2038 10% Glass Filled Nylon 6

PH0POL1469 / 146038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.