MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Domo TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This phosphorus and halogen free flame retardant grade is particularly suitable for equipment with robust glow wire resistance such as MCB housings. This grade is available in grey color.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
1.1 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0075 cm/cm0.0075 in/in
Linear Mold Shrinkage, Transverse 0.0112 cm/cm0.0112 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527 Type 1A
Elongation at Break 2.0 %2.0 %ISO 527 Type 1A
Tensile Modulus 6.13 GPa889 ksiISO 527 Type 1A
Izod Impact, Unnotched (ISO) 28.0 kJ/m²13.3 ft-lb/in²ISO 180/1eU
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
1210
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
1210
Glow Wire Ignition Temperature  700 °C
@Thickness 0.800 mm
1290 °F
@Thickness 0.0315 in
ISO 60695-2-13
 725 °C
@Thickness 1.60 mm
1340 °F
@Thickness 0.0630 in
ISO 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 220 - 230 °C428 - 446 °F
Front Barrel Temperature 245 - 255 °C473 - 491 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone230-240°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® 52G1MX 25 Grey 7035 PA6, Conditioned
Envalior Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond)
Envalior Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry)

PRHOD791 / 138022

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.