Plexiglas® V825-UVA5A is a thermoplastic acrylic resin formulated for injection molding and extrusion applications. It is formulated for specialty lighting packages requiring specific UV transmission requirements. Plexiglas® V825-UVA5A has excellent weatherability and optical properties allowing it to excel in applications requiring outdoor stability, high quality surface appearance and/or precision optics. Plexiglas® V825-UVA5A is easy to process due to its exceptional thermal stability, extrusion melt strength, and excellent tool surface reproduction and release properties. It has excellent resistance to many chemicals including solutions of inorganic acids, alkalis and aliphatic hydrocarbons such as VM&P naphtha and heptane. Additionally, it is virtually unaffected by a wide range of commercial products including many beverages, foodstuffs, detergent solutions and cleaners. Appearance: Clear/Transparent Characteristics: High Clarity; High Scratch Resistance; Good Dimensional Stability; Low Shrinkage; Good Thermal Stability, Good UV Stability; High Heat Resistance; Good Weather Resistance Applications: Automotive Applications; Lighting Diffusers; Optical Applications Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021. |