MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dover Chemical PAROIL 10NR Chlorinated Alkane, Extreme Pressure Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Paroil 10-NR is a medium chain chlorinated compound. It is a nonflammable, non-corrosive, low volatile liquid at room temperature. It contains a stabilizer to maintain product integrity during transport and storage. Paroil 10-NR is used in a wide variety of applications including flame retardants, plasticizers and EP metalworking packages. Paroil 10-NR is typically (but not limited to) used in machining operations.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc
@Temperature 25.0 °C
1.11 g/cc
@Temperature 77.0 °F
Density 1.11 g/cc0.0403 lb/in³
Viscosity 37 cP
@Temperature 25.0 °C
37 cP
@Temperature 77.0 °F
Saybolt Viscosity at 100°F 95 SUS95 SUS
Saybolt Viscosity at 210°F 35 SUS35 SUS
ASTM Color <= 0.50<= 0.50
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 180 °C>= 356 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 40 %40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER084 / 217703

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.