MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI Latistat 36/MR-04 ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Unfilled.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm0.0055 - 0.0075 in/in
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psi
Elongation at Break 2.5 %2.5 %
Elongation at Yield 2.0 %2.0 %
Tensile Modulus 3.10 GPa450 ksi
Charpy Impact Unnotched 1.00 J/cm²4.76 ft-lb/in²
Charpy Impact, Notched 0.120 J/cm²0.571 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 5000 ohm5000 ohm
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °F
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °F
Vicat Softening Point 100 °C
@Load 5.00 kg
212 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 70.0 - 80.0 °C
@Time 10800 sec
158 - 176 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLATH9975 / 177671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.