MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Atom Adhesives AA-SUPERTHERM 05 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-SUPERTHERM 05 is a thixotropic (smooth paste) Pure Diamond ultra-high thermally conductive epoxy two-part adhesive that develops strong, durable, high-impact bonds at room temperature which improve heat transfer while maintaining electrical insulation. AA-SUPERTHERM 05 bonds readily to itself, and to metals, silica, alumina, sapphire and other ceramics, glass, plastics and many other materials, because its coefficient of thermal expansion provides a good match for those materials over a fairly wide temperature range. Fully cured AA-SUPERTHERM 05 provides excellent resistance to salt solutions, mild acids and alkalis, and many other chemicals including petroleum solvents, lubricating oils, and alcohol. AA-SUPERTHERM 05 passes NASA`s outgassing specification making it ideal for demanding space applications.

Appearance: White

Cure Type: Heat cure or Room Temperature

Benefits:

  • Strong
  • Durable
  • High-impact bonds
  • Fullycured
  • Excellent resistance to many chemicals
Mix Ratio by weight: 100:100/Resin:Hardener

Substrates: metals, silica, alumina, sapphire and other ceramics, glass, plastics and many other materials

Typical Application: Extremely sensitive thermal cooling applications

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/ccmixed, uncured
Viscosity 33000 cP33000 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Izod Impact, Notched 0.262 J/cm0.490 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  3.20e+13 ohm-cm
@Temperature 75.0 °C
3.20e+13 ohm-cm
@Temperature 167 °F
 2.10e+15 ohm-cm
@Temperature 25.0 °C
2.10e+15 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 5.9
@Frequency 1000 Hz
5.9
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.9 µm/m-°C14.4 µin/in-°F
Thermal Conductivity 1.06 W/m-K7.36 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 115 °C239 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Glass Transition Temp, Tg 48.0 °C118 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Temperature 65.0 °C
2.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 45.0 min45.0 minuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PATOM037 / 172352

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.