Features: Excellent blend partner for PVC and general adhesive and good physical properties. Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating. Available in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |