MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SCG Chemicals H455JA High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: SCG HDPE H455JA is high density polyethylene resin with good process abiltiy, good mechanical property, and excellent organoleptic property. It is particularly designed for injection molding and continuous compression molding of caps and closures for the packaging beverages. Related Finished Products: Caps and closures for still and mineral water, juice, and tea.

Applications: Beverage caps and closures ( still and mineral water, juice and tea, hot filled beverages, aseptic beverages).

Features: Good process ability, good mechanical property, excellent organoleptic property.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 g/ccASTM D 1505
ESCR 10% Igepal® >= 7.0 hour
@Temperature 50.0 °C
Condition B, compression molded.; ASTM D1693
Linear Mold Shrinkage, Flow 0.0206 in/in
@Thickness 2.00 mm
TPE Method
Linear Mold Shrinkage, Transverse 0.0211 in/in
@Thickness 2.00 mm
TPE Method
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66ASTM D2240
Tensile Strength at Break 24.5 MPacrosshead speed 50 mm/min; ASTM D638
Tensile Strength, Yield 27.5 MPacrosshead speed 50 mm/min; ASTM D638
Elongation at Break 1250 %crosshead speed 50 mm/min; ASTM D638
Flexural Modulus 1230 MPaASTM D790
Izod Impact, Notched 39.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °CASTM D648
 
Descriptive Properties
AppearanceBlock pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC711 / 277968

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.