MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaowool 2000 Paper
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minimum. This specialty paper is noted for its excellent flexibility, outstanding handling characteristics, and high insulating value at high temperatures.

Features:

  • Very low thermal conductivity and heat storage
  • Extremely low (unifiberized material) content
  • Excellent high temperature parting agent
  • Thin, flexible high temperature insulation
  • Excellent tensile strength
  • Easily die cut for gasketing applications
  • Applications:

  • High temperature gaskets and seals
  • Refractory back-up insulation
  • Appliance insulation
  • Separating media for heat treating metals
  • High temperature filtration
  • High temperature expansion joint packing
  • Glassware separating media
  • Parting agent for brazing operations
  • Hot face and backup lining for lab furnaces
  • Aluminum distributor pan lining
  • Super alloy ingot mold lining and hot tapes.
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.176 - 0.224 g/cc0.00636 - 0.00809 lb/in³
    Loss On Ignition 6.0 - 10 %6.0 - 10 %
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 0.0345 - 0.0689 MPa5.00 - 10.0 psiFired
     >= 0.414 MPa>= 60.0 psi
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0548 W/m-K
    @Temperature 260 °C
    0.380 BTU-in/hr-ft²-°F
    @Temperature 500 °F
     0.0807 W/m-K
    @Temperature 538 °C
    0.560 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     0.115 W/m-K
    @Temperature 816 °C
    0.800 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
     0.160 W/m-K
    @Temperature 1090 °C
    1.11 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1180 °C2150 °F
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 47 %47 %
    SiO2 53 %53 %
     
    Descriptive Properties
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM243 / 2563

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.