Description: MTM55 is a controlled flow, 120°C (248°F) curing epoxy resin developed for autoclave, oven vacuum bag and press molding of components where exceptional surface quality is required. MTM55 exhibits enhanced toughness and is particularly suited to cosmetic applications and the sports good market. Features & Benefits: - 60 days out life at 21°C (70°F)
- 12 months storage at -18°C(0°F)
- Supplied on a range of lightweight surface plies and a limited range of heavier reinforcements
- Service temperature up to 90°C (194°F)
- Good tack and drape characteristic
- Exceptional surface quality
- Enhanced toughness
Information provided by Cytec, subsequently acquired by Solvay. |