MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Johnson Matthey Silver-flo™ 24 Silver Brazing Paste
Categories: Metal; Nonferrous Metal; Precious Metal; Solder/Braze Alloy

Material Notes: Silver-flo™ 24 brazing paste is a specially formulated paste product intended for use in semi- automated brazing processes or where the use of a paste offers other advantages. It combines Silver-flo™ 24, a comparatively high melting temperature silver brazing filler metal, in powder form with a flux-binder system selected to match an individual application. The resulting product is a fully dispensable custom-made brazing paste.

The use of a brazing paste can improve joint quality by helping to provide repeatability in the amount of filler metal and flux used. Using a brazing paste can lead to productivity improvements and well as enabling pre-placement of the brazing material which can reduce handling and waste.

Silver-flo™ 24 has a melting temperature of 740 to 800°C with a medium length melting range of 60°C providing moderate flow properties when molten. It can be used to fill gaps that cannot be tightly controlled. The optimum joint gap for this filler metal at brazing temperature is normally 0.075-0.2mm.

This filler metal has been incorporated into aviation / aero industry standards and is consequently used in the manufacture of components for applications in this field. It is also used as the first alloy in a two-step silver brazing operation, where the second joint is made with Silver-flo™ 55.

Silver-flo™ 24 can be used to join all the common engineering materials (excluding aluminum) such as copper, copper alloys (including, brasses, bronzes, gun metal, nickel silvers, aluminum bronze, copper nickel), steels including, mild, carbon, tool steel, stainless steels, low alloy steel). This alloy is not normally recommended for brazing tungsten carbide and PCD segments where Argo-braze™ silver brazing filler metals are often preferred.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 740 - 800 °C
Solidus 740 °C
Liquidus 800 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 43 %
Silver, Ag 24 %
Zinc, Zn 33 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Silver-flo™ 56 Cadmium Free Silver Brazing Paste
Johnson Matthey Silver-flo™ 452 Cadmium Free Silver Brazing Filler Metal
Nichrome 35-20 Medium Temperature Resistor Material
Johnson Matthey Copper-flo™ No. 3 Copper-Phosphorus Brazing Filler Metal
Johnson Matthey Argo-braze™ 502 Tri-foil Silver Brazing Filler Metal

NJMMJ9757 / 186158

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.