Radiation cross-linkable halogen-free, flame retardant insulation and sheathing compound. Compound class: Insulation / sheathing Compound category: RDX Flame retardant: ATH Standards: UL 1277 Oil Res II; IEEE1202 / CSA FT-4 Typical applications: The RDX 20521 compound is very low temperature resistant to – 40°C and IRM 902 & IRM 903 oil resistant Features: Flame retardant; Halogen-free; Low smoke; High temperature resistant; Oil resistant; Flexible; Flexible at low temperatures Information provided by Melos |