MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Caplinq LINQTAPE™ PET1S 1 mil polyester film with silicone adhesive
Categories: Polymer; Adhesive; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: LINQTAPE™ PET1S is a1-mil polyester film backing with a pressure sensitive silicone adhesive system. PET1S polyester tape is a no/low residue tape designed for splicing and masking applications where high initial adhesion is required, but no residue once the tape is removed. LINQTAPE™ PET1S is a high performance, flexible, polyester tape used in a wide range of applications. For very high temperature applications, polyimide tape should be used, but for applications with temperatures up to 204°C (400°F), PET1S can be used. These applications include but are not limited to splicing, masking and temporary bonding. LINQTAPE™ PET1S comes in 66meter (72yard) rolls of varying widths and is available in blue, yellow, red and green. LINQTAPEPET-S polyester films with silicone adhesive are available in a range of thicknesses, starting from 1mil (25.4µm) thickness and up. Custom thicknesses are available upon request.

Features& Applications:

  • High performance adhesive does not degrade in the presence of most chemicals and fumes
  • No adhesive residue after removal
  • Used in masking applications in the printed circuit board industry
  • Used for splicing applications on difficult to bond to surfaces, such as photo splicing
  • Powder coating and E-coating
  • Anodizing

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milFilm (Backing)
 43.2 microns1.70 milAdhesive
 68.6 microns2.70 milTotal
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 100 %>= 100 %
Tear Strength 5.34 kN/m30.5 plitensile, 1mil thick
Peel Strength 0.140 kN/m0.799 plito steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 165 kV/mm>= 4200 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 240 °C464 °F
 
Descriptive Properties
ColorBlue, Yellow, Red, Green
 Silicone
Insulation Class180 (H)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCAPL1012 / 256012

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.