MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyglycolic Acid (PGA)
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: This is a biodegradable polymer. It has been used in medical procedures as a wound closure material. It is generally formed and used with high crystallinity.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccCompletely Amorphous
 1.707 g/ccCompletely Crystalline
b Lattice Constant 6.19 Å
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 890 MPaFiber
Elongation at Break 30 %Fiber
Modulus of Elasticity 8.40 GPaFiber
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 191 J/gCompletely Crystalline
Melting Point 224 - 230 °C
Glass Transition Temp, Tg 36.0 - 40.0 °C
Decomposition Temperature 260 °C
 
Descriptive Properties
Unit CellOrthorhombic

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
Zeus Absorv® Poly(e-caprolactone) (PCL) Bioabsorbable Polymer
Zeus Absorv® Poly(L-lactide-co-glycolide), PLGA (85L/15G) Copolymer Bioabsorbable Polymer
Zeus Absorv® Poly(glycolide) (PGA) Bioabsorbable Polymer
Poly-L-lactide (PLLA)

P0BIO00 / 20044

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.