Varcum 29217 is a highly condensed, one-step, pulverized phenolic resin. APPLICATION: Formulating of brake blocks and brake linings. FEATURES: - Recommended for use in dry mix frictional formulations.
- Displays stable frictional characteristics under heavy duty braking conditions.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |