MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
DSM Somos® 9120
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Product Description: Somos® 9120 is a transparent stereolithography resin that is easy to use and fast to build. This stereolithography resin produces translucent, accurate parts that are semiflexible. Parts produced with Somos® 9120 exhibit excellent water and temperature resistance and mimic polypropylene. Somos® 9120 is ideal for applications such as fluid flow analysis, electrical casings and automotive parts. As this material is semi-flexible, it can also be used for snap-fit functional testing.

Key Benefits:

  • Highly transparent
  • Semi-flexible
  • Easy to use and finish
Ideal Applications
  • Automotive parts
  • Electrical casings
  • Fluid flow analysis

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Innovative leaders in producing high quality Rapid Prototyping and Rapid Manufacturing solutions using all major 3D printing systems including Stereolithography technology. Free online quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Viscosity 450 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81UV Postcure; ASTM D2240
Tensile Strength 31.0 MPaUV Postcure; ASTM D638M
Elongation at Yield 20 %UV Postcure; ASTM D638M
Tensile Modulus 1.35 GPaUV Postcure; ASTM D638M
Flexural Strength 45.0 MPaUV Postcure; ASTM D790M
Flexural Modulus 1380 MPaUV Postcure; ASTM D790M
Izod Impact, Notched 51.0 J/mUV Postcure; ASTM D256A
 
Descriptive Properties
AppearanceOff White
DP (mils)5.6Slope of cure-depth vs. ln (E) curve
E10 (mJ/cm2)65exposure that gives 0.254 mm (0.010 inch) thickness
Ec (mJ/cm2)10.9Critical Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems Accura® 60 Plastic for SLA® Systems
3D Systems Accura® 55 Plastic for SLA® Systems
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
3D Systems RenShape® SL 7820 Stereolithography Plastic

PDSM9886 / 161507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.