MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotch® 829 Packing List Pouch Tape
Categories: Polymer; Adhesive

Material Notes: Scotch® Packaging List Pouch Tape 829 is a pressure-sensitive tape with a red boarder framing a non-sticky, clear, rectangular center window, which allow attaching and protection of packing lists and other documents to boxes and shipping containers.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 30.5 microns1.20 milBacking; ASTM D3652
 48.3 microns1.90 milTotal; ASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 160 %160 %ASTM D3759
Peel Strength 0.438 kN/m2.50 pliAdhesion to Steel; ASTM D3330
Film Tensile Strength at Break, MD 7.55 MPa1100 psiASTM D3759
Film Tensile Strength at Break, TD 15.1 MPa2190 psiASTM D3759
 
Descriptive Properties
Adhesive TypePressure sensitive hot melt rubber-resin
AppearanceClear with red print

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch® 231A Performance Masking Tape
3M Scotch® 231 Performance Masking Tape
3M Scotch® 226 Solvent Resistant Masking Tape
3M Scotch® 222 High-temperature Fine Line Masking Tape
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape

PMM34219 / 168966

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.