MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mallard Creek Polymers Rovene® 4601 Carboxylated Styrene-Butadiene Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Rovene 4601 is a styrene-butadiene polymer emulsion designed to perform in textile applications. It may be utilized as a blend component, but may also find utility in textile applications where a very stiff final product is desired. Rovene 4601 can be compounded using calcium carbonate, clays and alumina trihydrate as fillers; sodium polyacrylate thickeners are commonly used to obtain the required application viscosity.

Markets: Textiles

Applications: Hand Modifier, Textile Backcoatings, Textile Coatings

Related Products: Rovene 6005, Rovene 6066, Rovene 9410, Rovene 6065, Rovene 6106, Rovene 4106

Information provided by Mallard Creek Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 51 - 53 %51 - 53 %
pH 6.5 - 8.06.5 - 8.0
Viscosity <= 500 cP<= 500 cP
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 42.0 °C108 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMCP9926 / 250428

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.