Fluon MFA 640 Series is a full range of color concentrates designed for use in medium flow MFA (perfluoromethylalkoxy) for pigmentation. The color concentrates are based on Hyflon® PFA 640 and are supplied in cylindrical pellet form. These pellets are approximately 0.080” long by 0.080” diameter. End Uses: Colored injection molded parts, film, tubing, colored wire or jacket insulation where a pigmented appearance is required. Information provided by AGC Chemicals Americas Inc. |